How can steels with poor machinability be machined?
Low-machinability steels (e.g. tool steels, quenched-and-tempered steels, martensitic stainless steels) are characterized by high toughness and a tendency to adhere to the tool. Machining requires tools with an ideal balance between hardness (to resist abrasion) and toughness (to avoid chipping). Multilayer coatings that thermally insulate the substrate are essential, as are cutting strategies that minimize work hardening.
Why do some steels have poor machinability in CNC machining?
The problem is the combination of hardness and ductility:
- Abrasion: Complex carbides in the alloy wear the tool flank.
- Adhesion: At low speeds, the material welds to the cutting edge.
- Forces: High spindle power is required and large forces are generated, deflecting long tools.
Which tools should be used for tough, difficult-to-machine steels?
“Problem Solver” tools:
- Substrate: Ultrafine grain (0.5-0.8 micron) with 10-12% cobalt for toughness.
- Geometry: Less-positive rake than for aluminum, but with controlled edge preparation (rounding) to protect the edge.
- Coating: AlTiN or TiSiN are standard choices.
How can premature wear be avoided when machining steels with poor machinability?
How to avoid premature wear:
- Climb Milling: Always.
- Cutting Speed (Vc): Not too low. If it is too low, built-up edge is promoted. Find the “sweet spot” (e.g. 80-120 m/min).
- Toolpath: Avoid restarting on sharp corners. Use radiused CAM toolpaths to keep load constant.