TTD1800330E

180° high-performance solid carbide pilot drill with reinforced shank, coated

d1m5d2h6d3+/-0.02l1+/-0.2l2+/-0.05l30/+0.2
3.36.04.860.011.616.8
CoatingYes
Coolant holesNo
Point angle180°
Flutes2
Chamfer45°
MaterialDescriptionMachinabilityVcm/minfnmm/rev
P.0Long chipping Low Carbon SteelsRecommended65-800.030-0.035
P.1Short chipping Low Carbon SteelsRecommended65-800.030-0.035
P.2Medium and High Carbon SteelsRecommended65-800.030-0.035
P.3Alloy Steels, Tool Steels (N/mm² 600-850)Recommended50-600.028-0.033
P.4Alloy Steels, Tool Steels (N/mm² 850-1400)Recommended40-500.028-0.033
P.5Ferritic, Martensitic, PH SSRecommended35-500.028-0.033
P.6High Strength Ferritic, Martensitic, PH SSRecommended35-500.014-0.016
M.1Austenitic Stainless SteelRecommended25-300.014-0.016
M.2High Strength Austenitic SS, Cast SSRecommended25-300.014-0.016
M.3Duplex SSRecommended25-300.014-0.016
K.1Grey Cast IronRecommended70-800.030-0.035
K.2Low and Medium Strength CGI, Ductile IronsRecommended60-700.030-0.035
K.3High Strength Ductile and Austempered Ductile IronRecommended60-700.030-0.035
N.1Wrought AluminiumPartially recommended115-1250.045-0.055
N.2Low Si Al Alloys and Magnesium Alloys Si<12%Partially recommended115-1250.045-0.055
N.3High Si Al Alloys Si>12%Partially recommended115-1250.045-0.055
N.4Copper, Brass, Zinc Based AlloysPartially recommended65-1000.028-0.055
S.1Iron Based HRSAPartially recommended15-200.012-0.013
S.2Co Based HRSAPartially recommended15-200.014-0.016
S.3Ni Based HRSAPartially recommended15-200.012-0.013
S.4Ti and Ti AlloysPartially recommended20-300.028-0.032
H.1Hardened Materials (HRC 44-48)Partially recommended15-200.012-0.013
H.2Hardened Materials (HRC 48-55)Partially recommended15-200.012-0.013
O.1Thermoplastic and thermosetting materialsPartially recommended115-1250.045-0.055