TMR2300600E

High-performance solid carbide ball nose end mill, coated

d1+/-0.01d2h6l1+/-0.2l20/+0.5l3-0/+1r0/-0.02
6.06.057.06.020.03.0
CoatingYes
Helix angle30°
Flutes2
StandardTUSA
MaterialDescriptionMachinabilityVcm/minfnmm/rev
P.0Long chipping Low Carbon SteelsRecommended80-1000.1875
P.1Short chipping Low Carbon SteelsRecommended80-1000.1875
P.2Medium and High Carbon SteelsRecommended80-1000.1875
P.3Alloy Steels, Tool Steels (N/mm² 600-850)Recommended60-800.1875
P.4Alloy Steels, Tool Steels (N/mm² 850-1400)Recommended50-700.1875
P.5Ferritic, Martensitic, PH SSRecommended50-700.1875
P.6High Strength Ferritic, Martensitic, PH SSRecommended50-700.1875
M.1Austenitic Stainless SteelRecommended50-700.1875
M.2High Strength Austenitic SS, Cast SSRecommended50-700.1875
M.3Duplex SSRecommended50-700.1875
K.1Grey Cast IronRecommended50-700.1875
K.2Low and Medium Strength CGI, Ductile IronsRecommended50-700.1875
K.3High Strength Ductile and Austempered Ductile IronRecommended50-700.1875
N.1Wrought AluminiumRecommended100-1200.1875
N.2Low Si Al Alloys and Magnesium Alloys Si<12%Recommended100-1200.1875
N.3High Si Al Alloys Si>12%Recommended100-1200.1875
N.4Copper, Brass, Zinc Based AlloysRecommended100-1200.1875
S.1Iron Based HRSARecommended30-500.1875
S.2Co Based HRSARecommended30-500.1875
S.3Ni Based HRSARecommended30-500.1875
S.4Ti and Ti AlloysRecommended30-500.1875
H.1Hardened Materials (HRC 44-48)Recommended40-600.1875
H.2Hardened Materials (HRC 48-55)Recommended30-500.1875
O.1Thermoplastic and thermosetting materialsRecommended100-1200.1875