How should Grade 5 titanium be drilled?
Grade 5 titanium (Ti-6Al-4V) has very low thermal conductivity: the generated heat remains concentrated at the tool tip and is not effectively dissipated into the chip or workpiece. Successful drilling therefore requires active heat removal. Drills with extremely sharp cutting edges are used to reduce friction and heat generation at the source, together with a moderate Vc (40-60 m/min). Chemistry also matters: titanium tends to react and adhere to the cobalt in carbide, so the coating must remain intact.
Which drills are recommended for drilling Grade 5 titanium?
K10/K20 carbide drills are recommended with:
- Grinding: Positive, sharp cutting edges (no heavy honing) to cut the metal cleanly.
- Polishing: Mirror-polished flutes to promote chip flow, since titanium chips tend to be gummy and pack together.
- No Double Margins: Prefer single-margin drills to reduce contact area and side friction.
Which parameters should be avoided to prevent titanium from overheating during drilling?
What not to do:
- Excessive Vc: Above 60-70 m/min, temperatures at the cutting edge can exceed > 800°C, triggering the titanium-tool chemical reaction and rapid crater wear.
- Uncertain/Too-Low Feed: Feeding too slowly causes work hardening and heat. Maintain a constant chip load.
- Insufficient Coolant: Flow must be abundant. Interruptions cause thermal shock and cracking at the drill tip.
How can clean holes be produced in titanium while reducing burrs and galling?
The objective is a hole within tolerance and a clean surface:
- Avoid Pecking: Titanium work hardens less than Inconel but is elastic. Each retraction risks the hole closing slightly on the drill. Continuous drilling is preferable.
- Exit Control: As with Inconel, slow down at exit so axial thrust does not create a tough burr that is difficult to remove.
- Fluid Quality: Use neat cutting oils or high-concentration emulsions (10%+) with EP (Extreme Pressure) additives.